To ALL,
This experiment was originally posted in the (general discussion section).
Evan if possible can you switch the original post to here ?
Well,
(6) wks has passed and here are my results.
ALL testing has been done by following the manufactures instructions and suggestions.
The product that I have been testing is (SHARKHIDE METAL PROTECTANT)some people have mentioned it before.
Supplies Used:
1. 100% virgin lacquer thinner (1)gallon
2. soft papertowels (lots)
3. Gerber babie diapers (flat fold style)
4. Sharkhide Metal protectant (2)qts
5. Sharkhide "Clint"(telephone consulting)
Test Results:
Sorry for no pictures (camera broke) but cary @ Camp-Inn has been sent some of the samples.
1. 292 continuous hours of (salt spraying) by a certified lab in Mass.
2. 1000 hrs of heat 95 deg
3. 1000 hrs of artificial sunlight with well/city water spray
4. Approx 750 hrs of pond water
5. approx 750 hrs of ocean salt water
6. approx 800 miles of road testing
7. bend test
As far as my results have proven this Sharkhide Metal Protectant WORKS (sharkhide.com) ask for Clint. I have tried to simmulate as best as I could but the decision is YOURS. As part of my results there is a very noticible difference between the protected side and the bare aluminum Un-protected side.
The metal shows water spots,white corrosion marks along the (brushed direction)of the surface and basic oxidizing of the aluminum. The protected side looks as new as the day I sealed it
You can do your own testing if you feel to do so but as far as I'am concerned I will be using this product and hopefully by then my camera will be fixed or replaced so I will be able to post some pictures of the samples and my CI. As far as I can see this product will outlast the woodys wax and Walbernize.
If you have any questions feel free to ask and I will try to answer but Clint @ sharkhide would be the person ask.
This experiment was originally posted in the (general discussion section).
Evan if possible can you switch the original post to here ?
Well,
(6) wks has passed and here are my results.
ALL testing has been done by following the manufactures instructions and suggestions.
The product that I have been testing is (SHARKHIDE METAL PROTECTANT)some people have mentioned it before.
Supplies Used:
1. 100% virgin lacquer thinner (1)gallon
2. soft papertowels (lots)
3. Gerber babie diapers (flat fold style)
4. Sharkhide Metal protectant (2)qts
5. Sharkhide "Clint"(telephone consulting)
Test Results:
Sorry for no pictures (camera broke) but cary @ Camp-Inn has been sent some of the samples.
1. 292 continuous hours of (salt spraying) by a certified lab in Mass.
2. 1000 hrs of heat 95 deg
3. 1000 hrs of artificial sunlight with well/city water spray
4. Approx 750 hrs of pond water
5. approx 750 hrs of ocean salt water
6. approx 800 miles of road testing
7. bend test
As far as my results have proven this Sharkhide Metal Protectant WORKS (sharkhide.com) ask for Clint. I have tried to simmulate as best as I could but the decision is YOURS. As part of my results there is a very noticible difference between the protected side and the bare aluminum Un-protected side.
The metal shows water spots,white corrosion marks along the (brushed direction)of the surface and basic oxidizing of the aluminum. The protected side looks as new as the day I sealed it
You can do your own testing if you feel to do so but as far as I'am concerned I will be using this product and hopefully by then my camera will be fixed or replaced so I will be able to post some pictures of the samples and my CI. As far as I can see this product will outlast the woodys wax and Walbernize.
If you have any questions feel free to ask and I will try to answer but Clint @ sharkhide would be the person ask.